Process for production of aromatic polycarbonate resin and molded article of aromatic polycarbonate resin
申请人:TEIJIN LIMITED
公开号:EP0995768A2
公开(公告)日:2000-04-26
An aromatic polycarbonate resin is produced under the conditions that the flow velocity of the reaction mixture in a pipe through which a molten reaction mixture passes is a specific value or over, the viscosity-average molecular weight of the reaction mixture is 1,000 or over, the sum of the average retention times of the reaction mixture is not longer than 3 hours, the wall temperature of the pipe through which a molten reaction mixture passes is set to be higher than the temperature of the reaction mixture in the pipe, the catalyst deactivation agent is added within 2 hours after the completion of the melt polycondensation reaction, the filtration is carried out by using a filter having a specific retained particle size under a specific pressure difference, specific treated amount of the aromatic polycarbonate resin per unit area of the filter and a ratio of W (flow quantity of filtered polymer) x 1,000/A (maximum area of the polymer path in the filtration vessel) falling within a specific range, etc.
The present invention provides a process for producing an aromatic polycarbonate resin and its molded article having excellent color and transparency as well as excellent color stability and thermal stability in high efficiency while suppressing contamination with foreign matters and the discoloration and gel formation of the resin.
芳香族聚碳酸酯树脂的生产条件是:熔融反应混合物通过的管道中反应混合物的流速为特定值或以上,反应混合物的粘度-平均分子量为 1,000 或以上,反应混合物的平均停留时间之和不超过 3 小时,熔融反应混合物通过的管道壁温设定为高于管道中反应混合物的温度、在熔融缩聚反应结束后 2 小时内加入催化剂失活剂,过滤时使用在特定压差下具有特定截留粒径的过滤器,过滤器单位面积上芳香族聚碳酸酯树脂的特定处理量以及 W(过滤聚合物的流量)×1,000/A(过滤容器中聚合物路径的最大面积)之比在特定范围内,等等。
本发明提供了一种生产芳香族聚碳酸酯树脂及其成型品的工艺,该工艺具有极佳的色泽和透明度,以及极佳的色稳定性和热稳定性,同时还能高效地抑制异物污染、树脂变色和凝胶的形成。