Thermoplastic elastomer composition, formed article and sealing material having low hardness
申请人:Kanae Kentarou
公开号:US20070173591A1
公开(公告)日:2007-07-26
A thermoplastic elastomer composition comprising the following components [A], [B], [C], and [D]: [A] 5 to 60 mass % of an ethylene-α-olefin-based copolymer having a limiting viscosity of 3.5 dl/g or more measured in a decalin solvent at 135° C., [B] 1 to 20 mass % of a polyolefin-based resin, and [C] 30 to 94 mass % of a mineral oil-based softening agent, provided that the total of the components [A], [B], and [C] is 100 mass %, and for 100 parts by mass of the components [A], [B], and [C], [D] 0.1 to 50 parts by mass of a hydrogenated diene-based polymer, at least [A] the ethylene-α-olefin-based copolymer and [B] the polyolefin-based resin being dynamically treated with heat in the presence of a cross-linking agent, or the above thermoplastic elastomer composition wherein [A] is replaced with an oil-extended rubber comprising [A1] 20 to 80 mass % of an ethylene-α-olefin-based copolymer having a limiting viscosity of 3.5 dl/g or more measured in a decalin solvent at 135° C. and [C1] 20 to 80 mass % of a mineral oil-based softening agent, provided that the total of [A1] and [C1] is 100 mass %. This thermoplastic elastomer composition excels in molding processability, has low hardness, is free from bleed-out of a mineral oil-based softening agent, has high flexibility and superior rubber elasticity (rebound resilience and compression set), and excels in recycling efficiency.
一种热塑性弹性体组合物,包括以下成分[A]、[B]、[C]和[D]:[A]占5至60质量%的乙烯-α-烯烃共聚物,其在135℃下在十二烷基溶剂中测量的极限粘度为3.5 dl/g或更高,[B]占1至20质量%的聚烯烃基树脂,[C]占30至94质量%的矿物油基软化剂,但要求成分[A]、[B]和[C]的总和为100质量%,并且对于成分[A]、[B]和[C]的100质量份,[D]占0.1至50质量份的氢化二烯基聚合物,其中至少成分[A]的乙烯-α-烯烃共聚物和成分[B]的聚烯烃基树脂在交联剂的存在下动态加热处理,或者将上述热塑性弹性体组合物中的[A]替换为扩展油橡胶,其包括[A1]占20至80质量%的乙烯-α-烯烃共聚物,其在135℃下在十二烷基溶剂中测量的极限粘度为3.5 dl/g或更高,以及[C1]占20至80质量%的矿物油基软化剂,但要求[A1]和[C1]的总和为100质量%。该热塑性弹性体组合物具有优异的成型加工性能,低硬度,不会出现矿物油基软化剂渗出,具有高柔韧性和优异的橡胶弹性(回弹弹性和压缩永久变形),且具有优异的回收利用效率。