There is provided a method for producing pigment crystals with sufficiently high purity and sufficiently controlled crystal type, particle size, and aggregation property and dispersibility to obtain a pigment crystal that can be suitably used in both a solid phase and a liquid phase. The method for producing pigment crystals (S3) from a pigment precursor (S0) using retro Diels-Alder reaction, the method comprising producing the pigment crystals (S3) from the pigment precursor (S0) through a first displacement structure (S1) and a second displacement structure (S2), which differ from the pigment precursor (S0) and the pigment crystals (S3) and also differ from at least from each other.
提供了一种生产
颜料晶体的方法,能够获得高纯度、控制晶体类型、粒径和聚集性以及分散性的
颜料晶体,以便在固态和液态中都能够适当使用。该方法通过反向Diels-Alder反应从
颜料前体(S0)生产
颜料晶体(S3),其中包括通过第一置换结构(S1)和第二置换结构(S2)从
颜料前体(S0)生产
颜料晶体(S3),这两种结构不同于
颜料前体(S0)和
颜料晶体(S3),并且至少彼此不同。