申请人:KUREHA KAGAKU KOGYO KABUSHIKI KAISHA
公开号:EP0369620A2
公开(公告)日:1990-05-23
Disclosed herein are a poly(arylene thioether) block copolymer alternately comprising (A) at least one poly-(arylene thioether-ketone) block having predominant recurring units of the formula
wherein the -CO- and -S- are in the para position to each other and (B) at least one poly(arylene thioether) block having predominant recurring units of the formula
(a) the ratio of the total amount of the poly(arylene thioether) block (B) to the total amount of the poly-(arylene thioether-ketone) block (A) being within a range of 0.05-5 by weight, (b) the average polymerization degree of the poly(arylene thioether) block (B) being at least 10, and (c) said block copolymer having a melt viscosity of 2-100,000 poises as measured at 350 C and a shear rate of 1,200/sec as well as a production process the poly(arylene thioether) block copolymer. The invention also provides a stabilized poly(arylene thioether) block copolymer containing a basic compound either alone or in combination with an antioxidant.
本文公开了一种聚(芳基硫醚)嵌段共聚物,它交替包含(A)至少一个聚(芳基硫醚酮)嵌段,该嵌段具有如下式的主要循环单元
其中-CO-和-S-互为对位,以及 (B) 至少一个具有式中主要递归单元的聚(芳基硫醚)嵌段
(a) 聚(芳基硫醚)嵌段(B)的总量与聚(芳基硫醚酮)嵌段(A)的总量之比为 0.(b) 聚(芳基硫醚)嵌段(B)的平均聚合度至少为 10,(c) 所述嵌段共聚物在 350℃和 1,200/sec 的剪切速率下测得的熔融粘度为 2-100,000 波,以及聚(芳基硫醚)嵌段共聚物的生产工艺。本发明还提供了一种稳定的聚芳基硫醚嵌段共聚物,其中含有一种碱性化合物,可以单独使用,也可以与抗氧化剂结合使用。