作者:Larry J. Markoski、Julie L. Thompson、Jeffrey S. Moore
DOI:10.1021/ma010980n
日期:2002.2.1
dendritic connectivities in the AB/AB2 copolymer products, was devised. By control of the stoichiometry and utiliziation of reaction conditions identical to those of the polymerizations, the products representing hyperbranched polymer units were produced and their ratios were monitored by 1H NMR and/or HPLC to indirectly determine the DB. In all reactions the A functionality was consumed in 2.5 min or
为了通过对支化度(DB)的系统研究将体系结构与物理性质联系起来,我们最近报道了一系列AB / AB 2单体的共聚反应,范围为0至1摩尔分数AB单体含量(x AB)。然而,由于严重的聚集和缺乏分散性,所以用标准的1 H NMR无法测量0.25 < x AB <1.0的共聚物的DB 。为了间接测量整个系列的DB,需要一个包含A,B和B 2官能度((A + B)/(A + B 2)模型反应)的不可聚合小分子的反应方案,其产物表示线性和AB中的树突状连接设计了2种共聚物产品。通过控制与所述聚合反应相同的化学计量和反应条件,产生了代表超支化聚合物单元的产物,并通过1 H NMR和/或HPLC监测它们的比率以间接测定DB。在所有反应中,A官能团在2.5分钟或更短的时间内就被消耗了(在2.5分钟内p A = 1),并且在任何一种分析技术中均未观察到可检测到的副产物。对于可测量的共聚物组成和相应的模型反应