Mouldable compositions comprising a metallic powder or a combination thereof with ceramic powder, mixed with an organic binder are disclosed, at least a part of which binder comprises a synthetic resin component (A) having a heat deformation temperature of 130°C or higher. The component A may be used in combination with another component (B) having a melting point of 30°C - 100°C, with or without another thermoplastic component (C), having a heat deformation temperature of 130°C or less. Mouldable compositions, comprising metallic and/or ceramic powder mixed with an organic binder comprising a secondary or tertiary amine (D), or a combination thereof with a thermoplastic resin (E), are also disclosed.
A polymer film comprising polyvinyl acetal and a laminated glass manufactured using the same are provided. The polymer film has a 45-100° C. dimensional variability ranging from 20 μm to 50 μm, and at least one surface of the polymer film has a surface roughness Rz ranging from 30 μm to 55 μm.
Polyvinylacetal-grafted polymers in the form of their aqueous dispersions or water-redispersible powders, and based on emulsion or suspension polymerized base polymers of one or more monomers from the group consisting of vinyl esters, (meth)acrylates, vinylaromatics, olefins, 1,3-dienes and vinyl halides, and optionally, further monomers copolymerizable therewith, the base polymers grafted with polyvinylacetals having from 0 to 5.0 mol % of vinyl acetate units, from 75 to 95 mol % of vinyl alcohol units and from 0.1 to 20 mol % of acetal units which are derived from aldehydes having 3 to 7 C atoms, are useful as additives in construction compositions, as binders, and as adhesives, and may be dried to form readily water-redispersible polymer powders.
BARBOT, F.;MIGINIAC, PH., SYNTHESIS, BRD, 1983, N 8, 651-654
作者:BARBOT, F.、MIGINIAC, PH.
DOI:——
日期:——
Optical film
申请人:KATO Shinya
公开号:US20080069975A1
公开(公告)日:2008-03-20
An optical film comprises: a transparent support; and a hardcoat layer comprising a heat- and/or ionizing radiation-curable resin and an organic resin particle having a refractive index of 1.60 or more, wherein a percentage change in an entire beam transmittance between before and after the optical film is exposed to an environment at a temperature of 80° C. and a relative humidity of 90% for 500 hours is 5% or less.