Preparation method of supercritical carbon dioxide thickener for tight oil and gas reservoir
申请人:Southwest Petroleum University
公开号:US11261373B2
公开(公告)日:2022-03-01
The present invention disclosed a method for preparing a thickener for tight oil and gas reservoir, which relieves damages. The technical solution includes the following steps: putting a three-flask in ice; adding perfluoroalkyl alcohol, P-toluenesulfonyl chloride and pyridine; reacting for 3 h at 0-20° C.; adding filter paper; ultrasonic dispersing for 1 h; removing the filter paper; washing the solution for 3-5 times by adding dilute hydrochloric acid to collect the intermediate product (I); adding 1,3-dihydroxy-propane-2-tert-butyl carbamate and the intermediate product (I) in another three-flask; adding potassium carbonate and N,N-dimethylformamide; reacting for 4 h at 40° C. to collect the intermediate product (II); adding trifluoroacetic acid and methylene chloride into the intermediate product (II); reacting at 45° C. for 2 h; extracting and vacuum drying; and adding 1,6-hexamethylene diisocyanate; reacting for 2 h to collect the final product (III).
本发明公开了一种用于致密油气藏的增稠剂的制备方法,该增稠剂可缓解损害。该技术方案包括以下步骤:将三口烧瓶放入冰中;加入全氟烷基醇、对甲苯磺酰氯和吡啶;在 0-20°C 下反应 3 小时。在另一个三口烧瓶中加入 1,3-二羟基丙烷-2-叔丁基氨基甲酸酯和中间产物 (I),加入碳酸钾和 N,N-二甲基甲酰胺,在 40°C 下反应 4 小时,收集中间产物 (II) 。在中间产物(II)中加入三氟乙酸和二氯甲烷,在 45 摄氏度下反应 2 小时,萃取并 真空干燥,然后加入 1,6-六亚甲基二异氰酸酯,反应 2 小时,得到最终产物(III)。