A polarizing plate protective film comprising a cellulose ester, and a saccharide ester compound in which all or a part of OH groups in Compound (A) or in Compound (B) are esterified, wherein Compound (A) consists of one of a furanose structure and a pyranose structure, and Compound (B) consists of two to twelve of at least one type of a furanose structure and a pyranose structure which are bonded in Compound (B); wherein the polarizing plate protective film exhibits Ro of 0-10 nm and Rt of −30 to +20 nm.
Cellulose ester film, polarizing plate and display
申请人:Murakami Takashi
公开号:US20070092663A1
公开(公告)日:2007-04-26
A cellulose ester film exhibiting: a free volume radius of 0.25 to 0.31 nm and a half-width of 0.04 to 0.1 nm, the free volume radius and the half-width being determined by positron annihilation lifetime spectroscopy; and Ro of 0 to 10 nm and Rt of −30 to ⇄20 nm, Ro and Rt being defined by the following equations: Equation (a): Ro=(nx−ny)×d; Equation (b): Rt=((nx+ny)/2−nz)×d (Ro: in-plane retardation, Rt: retardation in the thickness direction of the film, nx: in-plane refractive index in slow axis direction, ny: in-plane refractive index in fast axis direction, nz: refractive index in the thickness direction of the film (refractive indexes being measured at wavelength of 590 nm), d: thickness of the film (nm)).
METHOD FOR MANUFACTURING AN OPTICAL FILM HAVING A CONVEXOCONCAVE STRUCTURE, OPTICAL FILM, WIRE GRID POLARIZER AND RETARDATION FILM
申请人:SATO Akira
公开号:US20070252293A1
公开(公告)日:2007-11-01
A manufacturing method of an optical film provided with a convexoconcave structure, comprises the steps of: coating a resin solution including a first resin solved by a solvent onto an endless or roll-like mold provided with a convexoconcave structure, and forming a resin solution layer on the mold; laminating a film substrate onto the resin solution layer to make a laminated film before the solvent in the resin solution layer is completely dried, the film substrate including a second resin, which is capable of absorving the solution or is soluble by the solvent; and peeling the laminated film from the mold before the solvent in the laminated film is completely dried.
Cellulose Ester Film, Polarizing Plate and Display
申请人:Murakami Takashi
公开号:US20090202823A1
公开(公告)日:2009-08-13
A cellulose ester film exhibiting: a free volume radius of 0.25 to 0.31 nm and a half-width of 0.04 to 0.1 nm, the free volume radius and the half-width being determined by positron annihilation lifetime spectroscopy; and Ro of 0 to nm and Rt of −30 to +20 nm, Ro and Rt being defined by the following equations: Equation (a): Ro=(nx−ny)×d; Equation (b): Rt=((nx+ny)/2−nz)×d (Ro: in-plane retardation, Rt: retardation in the thickness direction of the film, nx: in-plane refractive index in slow axis direction, ny: in-plane refractive index in fast axis direction, nz: refractive index in the thickness direction of the film (refractive indexes being measured at wavelength of 590 nm), d: thickness of the film (nm)).
A cellulose acylate film is provided and contains an additive. Tg of the cellulose acylate film is lower by 5 to 50° C. or the half value width of the diffraction peak at 2θ=10 to 15° in the X-ray diffraction pattern of the cellulose acylate film after heating at 200° C. for 3 hours is 110 to 300%, each compared with a cellulose acylate film not containing the additive. An optically compensatory film, and a polarizing plate and a liquid crystal display using the film are provided.