A hydrogenated norbornene ring-open polymer obtained by hydrogenating 80% or more of main-chain carbon-carbon double bonds of a ring-open polymer which is obtained by ring-opening polymerization of 2-norbornene is disclosed. The hydrogenated norbornene ring-open polymer has a weight average molecular weight (Mw) determined by gel permeation chromatography (GPC) of 50,000 to 200,000, a molecular weight distribution (Mw/Mn) of 1.5 to 10.0, and a melting point of 110 to 145°C. Also disclosed is a hydrogenated norbornene ring-open polymer (hydrogenated polymer) obtained by hydrogenating 80% or more of carbon-carbon double bonds of a ring-open polymer which is obtained by ring-opening copolymerization of 2-norbornene and a substituent-containing norbornene monomer, wherein the proportion of a repeating unit (A) derived from the 2-norbornene with respect to all repeating units is 90 to 99 wt% and the proportion of a repeating unit (B) derived from the substituent-containing norbornene monomer with respect to all repeating units is 1 to 10 wt%. The hydrogenated ring-open polymer has a melting point of 110 to 145°C. A resin composition and a molding material containing these hydrogenated polymers, a molded article, a resin film, a resin sheet, a multilayer laminate, a packing material, a molded article for medical supplies, a blister molding sheet, a blister molded article, and a multilayer blow-molded container made of these hydrogenated polymers are also disclosed.
本发明公开了一种氢化
降冰片烯开环聚合物,该聚合物是通过氢化 2-
降冰片烯开环聚合得到的开环聚合物主链碳碳双键的 80% 或更多而得到的。氢化
降冰片烯开环聚合物的凝胶渗透色谱法(
GPC)测定的重量平均分子量(Mw)为 50,000 至 200,000,分子量分布(Mw/Mn)为 1.5 至 10.0,熔点为 110 至 145°C。本发明还公开了一种氢化
降冰片烯开环聚合物(氢化聚合物),它是通过氢化 2-
降冰片烯和含取代基
降冰片烯单体开环共聚得到的开环聚合物中 80%或更多的碳碳双键而得到的、其中由 2-
降冰片烯衍生的重复单元(A)占所有重复单元的比例为 90 至 99 wt%,由含取代基的
降冰片烯单体衍生的重复单元(B)占所有重复单元的比例为 1 至 10 wt%。氢化开环聚合物的熔点为 110 至 145°C。此外,还公开了含有这些氢化聚合物的
树脂组合物和成型材料、由这些氢化聚合物制成的成型品、
树脂薄膜、
树脂片材、多层层压板、包装材料、医疗用品成型品、吸塑成型片材、吸塑成型品和多层吹塑容器。