Method of preparing of 60% or more CIS-DI(C4-C20)alkyl cyclohexane-1,4-dicarboxylate
申请人:Hanwha Chemical Corporation
公开号:US08299292B2
公开(公告)日:2012-10-30
Provided is a method for preparing 60% or more cis-di(C4-C20)alkyl cyclohexane-1,4-dicarboxylate which exhibits superior plasticizing property for PVC resin. Instead of a phthalate- or terephthalate-based aromatic ester derivative, 60% or more cis-dimethyl cyclohexane-1,4-dicarboxylate is used as a starting material. The 60% or more cis-dimethyl cyclohexane-1,4-dicarboxylate is subjected to transesterification with (C4-C20) primary alcohol to prepare 60% or more cis-di(C4-C20)alkyl cyclohexane-1,4-dicarboxylate. Methanol produced as a byproduct during the transesterification is removed and some of the primary alcohol, which is evaporated, is recycled. Thus prepared 60% or more cis-di(C4-C20)alkyl cyclohexane-1,4-dicarboxylate exhibits superior plasticizer characteristics, including good plasticizing efficiency for PVC resin, high absorption rate, good product transparency after gelling, less bleeding toward the surface upon long-term use, and the like.
提供了一种制备60%或以上的顺式二(C4-C20)烷基环己烷-1,4-二羧酸酯的方法,该酯具有优异的PVC树脂增塑性能。该方法使用60%或以上的顺式二甲基环己烷-1,4-二羧酸酯作为起始物,而不是基于邻苯二甲酸酯或对苯二甲酸酯的芳香酯衍生物。将60%或以上的顺式二甲基环己烷-1,4-二羧酸酯与(C4-C20)一级醇进行酯交换反应,制备60%或以上的顺式二(C4-C20)烷基环己烷-1,4-二羧酸酯。在酯交换反应过程中产生的甲醇副产物被去除,并回收部分蒸发的一级醇。因此制备的60%或以上的顺式二(C4-C20)烷基环己烷-1,4-二羧酸酯具有优异的增塑性能,包括对PVC树脂的良好增塑效率、高吸收率、凝胶后良好的产品透明度、长期使用时少向表面渗出等特点。