An aromatic polycarbonate resin composition comprising:
100 parts by weight of a resin component consisting of (1) 50 to 100 wt% of an aromatic polycarbonate resin (component A) and (2) 0 to 50 wt% of at least one thermoplastic resin (component B) selected from the group consisting of a thermoplastic polyester resin (component B-1) and a styrene unit component-containing resin having a rubber component content of less than 40 wt% (component B-2); and
(3) 1 to 100 parts by weight of wollastonite particles having such particle shape characteristics that the particles have a number average fiber length measured by a method specified in this text of 10 µm or less and a number average fiber diameter measured by a method specified in this text of 4 µm or less and include particles having a fiber length of 5 to 25 µm in a number proportion of less than 50 % of the total
and moldings thereof.
According to the present invention, there are provided an aromatic polycarbonate resin composition which has high stiffness, high impact resistance, a good surface appearance (suppression of the formation of projecting foreign matter which causes deterioration in coating appearance) and recyclability, and moldings thereof.
芳香族聚
碳酸酯
树脂组合物,包括
100 份(按重量计)
树脂组分,包括:(1) 50 至 100 wt%的芳香族聚
碳酸酯
树脂 (组分 A)和 (2) 0 至 50 wt%的至少一种热塑性
树脂(组分 B),该热塑性
树脂选 自热塑性聚酯
树脂(组分 B-1)和橡胶组分含量低于 40 wt%的含
苯乙烯单元组分的
树脂(组分 B-2);以及
(3) 1 至 100 重量份的
硅灰石颗粒,其颗粒形状特征为:用本文规定的方法测得的 平均纤维长度数为 10 微米或以下,用本文规定的方法测得的平均纤维直径数 为 4 微米或以下,其中纤维长度为 5 至 25 微米的颗粒占总数的比例小于 50%; (4) 1 至 100 重量份的
硅藻土颗粒,其颗粒形状特征为:用本文规定的方法测得的 平均纤维长度数为 10 微米或以下,用本文规定的方法测得的平均纤维直径数 为 4 微米或以下,其中纤维长度为 5 至 25 微米的颗粒占总数的比例小于 50%。
及其成型品。
根据本发明,提供了一种芳香族聚
碳酸酯
树脂组合物,该组合物具有高硬度、高抗冲击性、良好的表面外观(抑制导致涂层外观恶化的凸出异物的形成)和可回收性,以及其模塑件。