VO43− species was synthesized. Several characterization techniques such as XRD, TEM, XPS, ESR, UV–vis DRS, V K-edge XAFS, 51V MAS NMR, Raman spectroscopy, and CO2 TPD revealed that the vanadium-apatite was Ca9(VO4)5(HVO4)(OH), abbreviated to VAP, covered with calcium oxide. This surface-coated calcium oxide phase could be removed by washing with water and then, the monomeric V-OH species having the strong
合成了含有VO 4 3-的
钒磷灰石。XRD,
TEM,XPS,ESR,UV-vis DRS,V K-edge XAFS,51 V MAS NMR,拉曼光谱和CO 2
TPD等几种表征技术表明,
钒磷灰石为Ca 9(VO 4)5(HVO 4)(OH),缩写为
VAP,用
氧化钙覆盖。可以通过用
水洗涤来除去该表面被覆的
氧化钙相,然后在
VAP的表面上生成具有强的布朗斯台德碱度的单体V-OH物质。固体
VAP催化的高效Michael反应在
水溶剂中具有很强的碱性。此外,发现
VAP适用于使用芳基
肼和
乙氧基亚甲基丙二酸二乙酯直接合成
吡唑啉酮衍
生物。