申请人:Kabushiki Kaisha Toshiba
公开号:EP3352253A1
公开(公告)日:2018-07-25
According to one embodiment, a nonaqueous electrolyte secondary battery includes a positive electrode, a negative electrode, and a nonaqueous electrolyte. The negative electrode includes a negative electrode current collector and a negative electrode mixed-material layer disposed on the negative electrode current collector. The negative electrode current collector includes a metallic foil. The negative electrode mixed-material layer includes a titanium-containing metal oxide having lithium ions inserted into and extracted from, and a binder that includes an acrylic resin. The negative electrode satisfies the following equation (I): α/β>1.36×10−2 In the equation, "α" represents a peel strength (N/m) between the current collector and the negative electrode mixed-material layer, and "β" represents a cutting strength (N/m) as measured according to a surface and interfacial cutting method in the negative electrode mixed-material layer.
根据一个实施方案,非水电解质二次电池包括正极、负极和非水电解质。负极包括负极集流器和设置在负极集流器上的负极混合材料层。负极集流器包括金属箔。负极混合材料层包括插入并提取锂离子的含钛金属氧化物,以及包括丙烯酸树脂在内的粘合剂。负极符合下式(I): α/β>1.36×10-2 式中,"α "表示集电体与负极混合材料层之间的剥离强度(N/m),"β "表示根据负极混合材料层表面和界面切割法测得的切割强度(N/m)。