A poly(ester-carbonate) copolymer comprises carbonate units of the formula (I); and ester units of the formula (II) wherein: T is a C2-20 alkylene, a C6-20 cycloalkylene, or a C6-20 arylene; and R1 and J are each independently (a) a bisphenol A divalent group and (b) a C16 or higher divalent group (b), wherein the C16 or higher divalent group is present in an amount of 40 to 50 mol %; the ester units are present in an amount of 40 to 60 mol %; the poly(ester-carbonate) copolymer has a weight average molecular weight of 18,000 to 24,000 Daltons; and a sample of the composition has a glass transition temperature of 210° C. to 235° C. as determined by differential scanning calorimetry (DSC) as per ASTM D3418 with a 20° C./min heating rate; and a melt viscosity of less than 1050 Pa-s at 644 sec-1 and 350° C., determined according to ISO 11443.
一种聚(酯-
碳酸酯)共聚物由式(I)的
碳酸酯单元和式(II)的酯单元组成,其中:T是C2-20亚烷基、C6-20环亚烷基或C6-20芳基;R1和J各自独立地是(a)
双酚A二价基团和(b)C16或更高二价基团(b),其中C16或更高二价基团的含量为40至50摩尔%;酯单元的含量为 40 至 60 摩尔%; 聚(酯-
碳酸酯)共聚物的重量平均分子量为 18,000 至 24,000 道尔顿; 组合物样品的
玻璃化转变温度为 210 摄氏度至 235 摄氏度。根据 ASTM D3418 以 20° C./min 的加热速率通过差示扫描量热法 (
DSC) 测定,
玻璃化转变温度为 210° C.至 235°C.;在 644 秒-1 和 350° C.条件下,熔融粘度小于 1050 Pa-s、根据 ISO 11443 测定。