A recording material includes applying a first ink including a first polymerizable compound using an inkjet method, polymerizing the first polymerizable compound using ultraviolet light irradiation to form a first layer, applying a second ink containing a second polymerizable compound and metal powder on the area on which the first layer is formed using the inkjet method, and polymerizing the second polymerizable compound using ultraviolet light irradiation to form a second layer. An deposition volume of the first ink in the area is 2.0 to 20.0 g/m2. A time from landing of the first ink droplets until ultraviolet light irradiation is 0.0010 to 1.0 second. An deposition volume of the second ink in the area is 80 to 200 volume % compared to the deposition volume of the first ink. A time from landing of the second ink droplets untilultraviolet light irradiation is 5.0 to 60.0 seconds.
一种记录材料包括使用喷墨方法涂抹包含第一可聚合化合物的第一墨
水,使用紫外线照射聚合第一可聚合化合物以形成第一层,使用喷墨方法在形成第一层的区域涂抹包含第二可聚合化合物和
金属粉末的第二墨
水,使用紫外线照射聚合第二可聚合化合物以形成第二层。第一层墨
水在该区域的沉积量为 2.0 至 20.0 克/平方米。从第一墨滴降落到紫外线照射的时间为 0.0010 至 1.0 秒。与第一种油墨的沉积量相比,第二种油墨在该区域的沉积量为 80 至 200 体积%。从第二墨滴降落到紫外线照射的时间为 5.0 至 60.0 秒。