An aromatic polycarbonate resin composition is obtained by removing a solvent from a resin solution that is obtained by dissolving an aromatic polycarbonate resin-A that has a viscosity-average molecular weight of 3,000-25,000 and an aromatic polycarbonate resin-B that has a viscosity-average molecular weight of 50,000-90,000 into the solvent. The aromatic polycarbonate resin-A is contained in an amount of 99-50% by mass and the aromatic polycarbonate resin-B is contained in an amount of 1-50% by mass relative to the total mass of the aromatic polycarbonate resin-A and the aromatic polycarbonate resin-B; a plate-like molded article having thickness of 3.0 mm and molded from the aromatic polycarbonate resin composition has a haze value of 2% or less; and the number of unmelted polycarbonate pieces having a length of 100 μm or more and present within a region of 5 cm×3 cm in the plate-like molded article is 10 or less.
一种芳香族聚
碳酸酯
树脂组合物的制备方法,包括从
树脂溶液中去除溶剂。所述
树脂溶液是通过将具有粘度平均分子量为3,000-25,000的芳香族聚
碳酸酯
树脂-A和具有粘度平均分子量为50,000-90,000的芳香族聚
碳酸酯
树脂-B溶解到溶剂中得到的。所述芳香族聚
碳酸酯
树脂-A的含量相对于芳香族聚
碳酸酯
树脂-A和芳香族聚
碳酸酯
树脂-B的总质量为99-50% ,所述芳香族聚
碳酸酯
树脂-B的含量相对于芳香族聚
碳酸酯
树脂-A和芳香族聚
碳酸酯
树脂-B的总质量为1-50%。用该芳香族聚
碳酸酯
树脂组合物制成的厚度为3.0毫米的板状成型品的浑浊度值为2%或以下;在板状成型品的5厘米×3厘米区域内,长度为100微米或更长的未熔化聚
碳酸酯碎片的数量为10个或以下。