Ni particles and Ni3C whiskers with a novel morphology, grew on the Ni–carbon composite by heat treatment at 1073 K in Ar. Ni–carbon composites were prepared by spray pyrolysis of a solution of sucrose and NiSO4 in Ar at 1073 K.
在氩气中于 1073 K 进行热处理后,镍-碳复合材料上生长出了具有新颖形态的镍颗粒和镍-3C 晶须。镍-碳复合材料是通过在 1073 K 的氩气中对蔗糖和 NiSO4 溶液进行喷雾热解制备的。
Cobalt(II) cyanide and its complexes with water, ammonia and cyanide ions