Provided is a producing method for a retardation film with a reverse wavelength dispersion property, which is highly reliable in terms of a small wavelength dispersion change and is low in display unevenness due to a position dependence of a retardation variation. The production method is designed for a retardation film which satisfies the following formulas (1) and (2): 0.7