There is provided a process for producing a modified polypropylene resin, which comprises the steps of mixing the following components (A) to (D), and reacting them with one another:
(A) 100 parts by weight of a polypropylene resin,
(B) 0.1 to 30 parts by weight of a compound having a bond or a functional group selected from the group consisting of a non-aromatic carbon-carbon multiple bond, an oxirane group and a derived carboxyl group,
(C) 0.001 to 30 parts by weight of a compound having at least two functional groups reactive to a carboxyl group, and
(D) 0.01 to 20 parts by weight of an organic peroxide having a decomposition temperature of from 50 to 120° C., at which temperature a half-life of the organic peroxide is 1 minute.
本发明提供了一种生产改性聚丙烯树脂的工艺,该工艺包括以下步骤:混合以下组分(A)至(D),并使其相互反应:
(A) 100 重量份的聚丙烯树脂、
(B) 0.1 至 30 份(按重量计)具有从非芳香族碳-碳多键、环氧乙烷基团和衍生 羧基组成的组中选出的键或官能团的化合物、
(C) 0.001 至 30 份(重量)具有至少两个与羧基反应的官能团的化合物,及
(D) 0.01 至 20 份(按重量计)有机过氧化物,其分解温度为 50 至 120 摄氏度,在此温度下,有机过氧化物的半衰期为 1 分钟。