申请人:PHILLIPS PETROLEUM COMPANY
公开号:EP0534359A1
公开(公告)日:1993-03-31
A process for preparing arylene sulfide polymers which comprises the steps of contacting at least one first alkali metal aminoalkanoate with a molar excess relative to the aminoalkanoate of hydrogen sulfide in an enclosed reaction vessel under reaction conditions of time and temperature sufficient to react the hydrogen sulfide with the first alkali metal aminoalkanoate to produce alkali metal bisulfide and thereby form a first reaction product comprising hydrogen sulfide, alkali metal bisulfide, water and lactam, venting the enclosed reaction vessel to remove hydrogen sulfide present in the first reaction product, contacting the alkali metal bisulfide with at least one second alkali metal aminoalkanoate under reaction conditions of time and temperature sufficient to produce a second reaction product comprising water, lactam and a polymerizable complex of the second alkali metal aminoalkanoate and the alkali metal bisulfide, dehydrating the second reaction product, contacting the dehydrated second reaction product with at least one dihaloaromatic compound to form a polymerization mixture, and subjecting the polymerization mixture to polymerization conditions of time and temperature sufficient to produce the arylene sulfide polymer.
一种制备芳基硫醚聚合物的工艺,包括以下步骤:在封闭的反应容器中,在反应时间和温度足以使硫化氢与第一碱金属氨基烷酸酯反应生成碱金属硫化氢的条件下,使至少一种第一碱金属氨基烷酸酯与相对于氨基烷酸酯摩尔过量的硫化氢接触,从而形成由硫化氢、碱金属硫化氢、水和内酰胺组成的第一反应产物,排出封闭的反应容器以除去存在于第一反应产物中的硫化氢、在足够的时间和温度反应条件下,将碱金属硫化氢与至少一种第二碱金属氨基烷酸酯接触,以产生由水、内酰胺和第二碱金属氨基烷酸酯与碱金属硫化氢的可聚合复合物组成的第二反应产物,使第二反应产物脱水,将脱水的第二反应产物与至少一种二卤代芳香族化合物接触,以形成聚合混合物,并使聚合混合物在足够的时间和温度条件下聚合,以产生芳基硫醚聚合物。