PROCESS FOR PRODUCING FLUORINE-CONTAINING COPOLYMER COMPOSITION AND FLUOROCARBON-RESIN MOLDED PRODUCT
申请人:Asahi Glass Company, Limited
公开号:EP2559730A1
公开(公告)日:2013-02-20
To provide a process for producing an ethylene/tetrafluoroethylene copolymer composition which is excellent in mechanical properties of the molded product and which has good moldability. A process for producing a fluorinated copolymer composition, which comprises heating a mixture (D) comprising a high molecular weight fluorinated copolymer (A) having repeating units derived from tetrafluoroethylene and repeating units derived from ethylene and having a melt viscosity of from 1,500 to 35,000 Pa·s at a temperature higher by 15°C than the melting point, a fluorinated copolymer (B) having a molecular weight lower than the fluorinated copolymer (A), having repeating units derived from tetrafluoroethylene and repeating units derived from ethylene and having a melt viscosity of from 50 to 3,000 Pa·s at a temperature higher by 15°C than the melting point, said melt viscosity of the fluorinated copolymer (B) being at most 1/5 of the melt viscosity of the fluorinated copolymer (A) at a temperature higher by 15°C than the melting point of the fluorinated copolymer (A), and a solvent (C) capable of dissolving the fluorinated copolymer (A) and the fluorinated copolymer (B) at a temperature not higher than the melting points of the fluorinated copolymer (A) and the fluorinated copolymer of (B), to at least a temperature where the fluorinated copolymer (A) and the fluorinated copolymer (B) are dissolved in the solvent (C) to obtain a solution state; and removing the solvent (C).
提供一种生产乙烯/四氟乙烯共聚物组合物的工艺,该组合物在模塑产品的机械性能方面非常优异,并且具有良好的可模塑性。一种生产含氟共聚物组合物的工艺,包括加热由高分子量含氟共聚物(A)组成的混合物(D),该共聚物具有来自四氟乙烯的重复单元和来自乙烯的重复单元,熔融粘度为 1,500 至 35、在温度比熔点高 15°C 时,熔体粘度为 1,500 至 35,000 Pa-s;氟化共聚物 (B),其分子量低于氟化共聚物 (A),具有从四氟乙烯衍生的重复单元和从乙烯衍生的重复单元,在温度比熔点高 15°C 时,熔体粘度为 50 至 3、氟化共聚物(B)的熔体粘度最多为氟化共聚物(A)熔体粘度的 1/5(温度比氟化共聚物(A)的熔点高 15°C)、以及能够在不高于氟化共聚物(A)和氟化共聚物(B)熔点的温度下溶解氟化共聚物(A)和氟化共聚物(B)的溶剂(C),至少达到氟化共聚物(A)和氟化共聚物(B)溶解在溶剂(C)中得到溶液状态的温度;并移除溶剂 (C)。