This invention is related to a process for preparing polyester polymers using a composite catalyst comprises the steps of 1) esterifying naphthalene dicarboxylic acid or a dicarboxylic acids containing NDCA or ester derivatives thereof, with ethylene glycol or glycols containing ethylene glycol or derivatives thereof to produce esterified compounds or its low molecular weight polymers; and then 2) continuously polycondensing the obtained esterification product to produce polyester polymers; and wherein the process includes using a composite polymerization catalyst which was prepared by reacting titanium compounds and cobalt compounds in the solution containing at least one alcohol. The process yields high quality polyester polymers having a good color and excellent physical properties. The process can considerably reduce both the esterification time and the polycondensation time.
本发明涉及一种使用复合催化剂制备聚酯聚合物的工艺,包括以下步骤:1)将
萘二
羧酸或含有 NDCA 的二
羧酸或其
酯类衍
生物与
乙二醇或含有
乙二醇的
乙二醇或其衍
生物酯化,生成酯化化合物或其低分子量聚合物;然后 2)将获得的酯化产物连续缩聚,生成聚酯聚合物;其中该工艺包括使用复合聚合催化剂,该催化剂是通过
钛化合物和
钴化合物在含有至少一种醇的溶液中反应制备的。该工艺可制备出具有良好色泽和优异物理性能的高品质聚酯聚合物。该工艺可大大缩短酯化时间和缩聚时间。