The object of the present invention is to provide a method for producing a (meth)acryloyl-terminated polyisobutylene polymer in which the auxiliary material used in the manufacture is easily removed, the burden of purification step and waste amount are decreased, and the transparency of the polymer is excellent. The method for producing the (meth)acryloyl-terminated polyisobutylene polymer contains a step 1 of polymerizing an isobutylene monomer under the presence of a Lewis acid catalyst to prepare a halogen-terminated polyisobutylene polymer (B), a step 2 of reacting the halogen-terminated polyisobutylene polymer (B) with a compound (C) having a halogen group and a phenoxy group under the presence a Lewis acid catalyst to prepare a halogenated phenoxyalkyl-terminated polyisobutylene polymer (D), and a step 3 of reacting the halogenated phenoxyalkyl-terminated polyisobutylene polymer (D) with an acrylic acid compound (E) to prepare the (meth)acryloyl-terminated polyisobutylene polymer (A).
本发明的目的是提供一种生产(甲基)丙烯酰基封端的聚异丁烯聚合物的方法,该方法易于去除生产中使用的辅助材料,减少了纯化步骤的负担和废物量,并且聚合物的透明度极佳。(甲基)丙烯酰基封端聚异丁烯聚合物的生产方法包括步骤 1:在路易斯酸催化剂存在下聚合异丁烯单体,制备卤素封端聚异丁烯聚合物 (B)、步骤 2:在路易斯酸催化剂存在下,将卤素封端聚异丁烯聚合物(B)与具有卤素基和苯氧基的化合物(C)反应,制备卤代苯氧基烷基封端聚异丁烯聚合物(D),步骤 3:将卤代苯氧基烷基封端聚异丁烯聚合物(D)与丙烯酸化合物(E)反应,制备(甲基)丙烯酰基封端聚异丁烯聚合物(A)。