[EN] METHOD OF PINE WOOD IMPREGNATION<br/>[FR] PROCÉDÉ D'IMPRÉGNATION DU BOIS DE PIN
申请人:EURO LOGISTICS GROUP SP Z O O
公开号:WO2020214040A1
公开(公告)日:2020-10-22
The method of pine wood impregnation by vacuum-pressure saturation with a solution of chromium-free, salt wood preservative based on inorganic copper and boron compounds as well as organic components where a negative pressure is generated in the first phase, the second one fills the autoclave with a impregnant, the third creates a pressure of several bars, which pushes the impregnate deep into the wood and then atmospheric pressure is restored and the autoclave has a vacuum and excess impregnation is removed from the wood surface is characterized by the fact that the wood is subjected to vacuum-pressure solution of a chromium-free, salt wood preservative based on inorganic copper compounds (copper-based HDO) and boron and organic ingredients called Wolmanit CX-10 with the addition of ionic liquid (DDA) (N03) at a concentration of 3.5% with 3.0% by weight, under negative pressure (0.7 ± 0.1) kPa, during 60 minutes, and atmospheric pressure during 120 minutes, at a temperature of 20 ± 1 ° C). For pressure impregnation, wood with a maximum moisture content of up to 28% is used. Retention of Wolmanit CX-10 in the wood of pine samples Pinus sylvestris L. saturated with the cold bath method - 20 ± 1 0 C, lasts 6 hours with Wolmanit CX-10 solution at a concentration of 3.5% by weight or Wolmanit CX-10 solution at a concentration of 3, 5% with 3.0% by weight with the addition of ionic liquid [DDA] [N03]. Quaternary ammonium salt penetrates into sapwood similar to copper penetration with saturation with Wolmanit CX-10 solution with the addition of [DDA] [N03], and in heartwood this salt penetrates more than twice as deep as copper.