A method of treating polyester fibers, which comprises
(1) treating the polyester fibers with an adhesive composition (AR) comprising a latex (A) of a vinylpyridine/conjugated diene copolymer having a vinylpyridine unit content of at least 20 % by weight but not more than 70 % by weight and a resorcinol-formaldehyde resin as main components, and
(2) further treating it with an adhesive composition (BR) comprising a latex (B) of a nitrile group-containing highly saturated copolymer rubber having an iodine number of not more than 120 and a resorcinolformaldehyde resin as main components.
A composite obtained by bonding the treated polyester fibers to a nitrile group-containing highly saturated copolymer rubber by vulcanization has high initial and heat-resistant adhesion strength, and is useful for production of timing belts and polyribbed belts.
一种处理聚酯纤维的方法,其中包括
(1) 用粘合剂组合物(AR)处理聚酯纤维,该组合物包括
乙烯基吡啶/共轭二烯共聚物胶乳(A),其
乙烯基吡啶单元含量至少为 20%(重量)但不超过 70%(重量),以及
间苯二酚-
甲醛树脂作为主要成分,以及
(2) 进一步用粘合剂组合物 (BR) 对其进行处理,粘合剂组合物 (BR) 的主要成分包括
碘数不超过 120 的含腈基高度饱和共聚橡胶的胶乳 (B) 和
间苯二酚甲醛树脂。
通过
硫化将处理过的聚酯纤维与含腈基团的高饱和共聚橡胶粘合在一起而得到的复合材料具有较高的初始粘合强度和耐热粘合强度,可用于生产同步带和多楔带。