申请人:General Electric Company
公开号:EP1854823A1
公开(公告)日:2007-11-14
A method for making a copolymer polyimide resin. The method includes providing a first prepolymer component and a second prepolymer component. The first prepolymer component has the formula, E1-[R1]n-E1 and the second prepolymer component has the formula E2-[R2]n-E2, M1, or a combinations thereof. R1 and R2 have the formula:
In the formulae, n is from about 1 to about 4; V is a tetravalent aromatic monocyclic or polycyclic linking structure; R is a divalent organic radical; E1 and E2 include crosslinkable functional groups. M1 includes a mixture of compounds selected from the group consisting of diamine compounds, dianhydride compounds, end group compounds, and combinations thereof. The process further includes blending the first and second prepolymer components to form a prepolymer mixture having a glass transition temperature of the mixture greater than about 450° F or the melt viscosity of the mixture less than about 1000 centipoise.
一种制造共聚聚酰亚胺树脂的方法。该方法包括提供第一种预聚物组分和第二种预聚物组分。第一种预聚物组分的化学式为 E1-[R1]n-E1,第二种预聚物组分的化学式为 E2-[R2]n-E2、M1 或其组合。R1 和 R2 的化学式为
式中,n 为约 1 至约 4;V 为四价芳香族单环或多环连接结构;R 为二价有机基;E1 和 E2 包括可交联官能团。M1 包括选自二胺化合物、二酸酐化合物、端基化合物及其组合的化合物混合物。该工艺还包括混合第一和第二种预聚物组分,以形成一种预聚物混合物,该混合物的玻璃化转变温度大于约 450 华氏度,或该混合物的熔融粘度小于约 1000 厘泊。