A polycarbonate resin composition comprising a polycarbonate resin and 0.001 to 1 parts by weight of an N-R type (R represents an alkyl group) hindered amine-based optical stabilizer per 100 parts by weight of the polycarbonate resin, wherein the polycarbonate resin comprises 40 mol% or more of a recurring unit (A) represented by the following formula and satisfies the following formulas (i) to (v), and the resin composition has excellent heat resistance, a low water absorption coefficient and high transparency, and suppresses deterioration during long-term use:
(i) a metal compound comprising a negative ion represented by the following formula (B) and a positive ion constituted by a metal is used as a polymerization catalyst in an amount of 1 × 10-9 to 1 × 10-5 molar equivalent relative to the total diol compounds used for polymerization;
(ii) the specific viscosity measured with a methylene chloride solution at 20°C is 0.23 to 0.60;
(iii) the glass transition temperature is 100°C to 160°C;
(iv) the saturated water absorption coefficient is 2.5% or less; and
(v) the relationship between the glass transition temperature (Tg°C) and the saturated water absorption coefficient (Wa%) satisfies the following formula (I): 2.5≤Tw value=Tg×0.04−Wa wherein R1 is an alkylene group, a cycloalkylene group, or an arylalkylene group which has 1 to 22 carbon atoms and may be linear or branched.
一种聚
碳酸酯
树脂组合物,包括聚
碳酸酯
树脂和每 100 份聚
碳酸酯
树脂重量含 0.001 至 1 份 N-R 型(R 代表烷基)受阻胺基光学稳定剂,其中聚
碳酸酯
树脂包含 40 摩尔%或更多由下式表示的循环单元(A),并满足以下公式(i)至(v),且该
树脂组合物具有优异的耐热性、低吸
水系数和高透明度,并在长期使用过程中抑制劣化:
(i) 使用由下式(B)表示的负离子和
金属构成的正离子组成的
金属化合物作为聚合催化剂,其用量相对于用于聚合的二元醇化合物总量为 1 × 10-9 至 1 × 10-5 摩尔当量;
(ii) 在 20°C 時以
二氯甲烷溶液測得的比黏度為 0.23 至 0.60;
(iii)
玻璃化转变温度为 100°C 至 160°C
(iv) 饱和吸
水系数为 2.5%或更低;以及
(v)
玻璃化转变温度(Tg°C)与饱和吸
水系数(Wa%)之间的关系满足下式(I):2.5≤Tw 值=Tg×0.04-Wa 其中,R1 是烷基、环烷基或芳基烷基,具有 1 至 22 个碳原子,可以是直链或支链。