The present invention relates to the technical field of chemical fiber spinning, in particular to a process for preparing an ultra-high-count filament yarn of PI-PSA electrospun fiber and uses thereof, the process comprises the steps of: step 1: after a monomer (I) and a monomer (II) are purified, adding the monomer (I) and monomer (II) to a polymerization reactor together with a solvent to obtain a polyamic acid solution, which is then mechanically mixing the polyamic acid solution with a PSA to obtain a spinning raw material liquid of the polyamic acid and the PSA; step 2: implementing electrostatic spinning to the spinning raw material liquid in a high-voltage electric field, and collecting to obtain a felt or nonwoven fabric of polyamic acid/PSA electrospun fibers using a stainless steel mesh belt as a collector; step 3: cutting the felt or nonwoven fabric of polyamic acid/PSA electrospun fibers obtained above into slender strips with a width of 0.5 to 5.0 cm, and thermally drafting and imidizing the strips to form an oriented electrospun fiber bundle; step 4: twisting the above electrospun fiber bundle to obtain an ultra-high-count filament yarn of PI-PSA electrospun composite fiber.
本发明涉及化纤纺丝技术领域,尤其涉及一种
PI-P
SA 电纺丝超高支长丝的制备工艺及其用途,该工艺包括以下步骤: 步骤 1:单体(I)和单体(II)提纯后,将单体(I)和单体(II)与溶剂一起加入聚合反应器中,得到聚酰胺酸溶液,然后将聚酰胺酸溶液与P
SA机械混合,得到聚酰胺酸和P
SA的纺丝原料液;步骤2:步骤 2:在高压电场中对纺丝原料液进行静电纺丝,并用不锈钢网带作为收集器进行收集,得到聚
氨基酸/P
SA 电纺纤维毡或无纺布;步骤 3:将上述得到的聚
氨基酸/P
SA 电纺纤维毡或无纺布切割成宽度为 0.5至5.0厘米的细条,并对细条进行热牵伸和
酰亚胺化处理,形成取向电纺纤维束;步骤4:对上述电纺纤维束进行加捻,得到
PI-P
SA电纺复合纤维超高支长丝。