PROPYLENE POLYMER, PROCESS FOR PRODUCING THE SAME, COMPOSITION CONTAINING THE SAME, AND USE THEREOF
申请人:Japan Polypropylene Corporation
公开号:EP2177544A1
公开(公告)日:2010-04-21
A propylene-based polymer which is suitably applicable to foam molding, sheet molding, blow molding or the like, because of having good flow characteristics, high melt tension, high swell ratio and thus good molding workability.
It is attained by a propylene-based polymer or the like characterized by satisfying the following requirements (i) to (vi).
Requirement (i): MFR is 0.1 g/10 minutes to 100 g/10 minutes.
Requirement (ii): Q value by GPC is 3.5 to 10.5.
Requirement (iii): ratio of components with a molecular weight of equal to or higher than 2, 000,000, in a molecular weight distribution curve obtained by GPC, is equal to or larger than 0.4% by weight and less than 10% by weight.
Requirement (iv): components, which elute at a temperature of equal to or lower than 40°C, are equal to or less than 3.0% by weight, in temperature rising elution fractionation by ODCB.
Requirement (v): isotactic triad fraction (mm) measured with 13C-NMR is equal to or higher than 95%.
Requirement (vi): strain hardening degree (λmax), in measurement of extensional viscosity, is equal to or higher than 6.0.
一种丙烯基聚合物,由于具有良好的流动特性、高熔体张力、高溶胀比,因此具有良好的成型加工性,可适用于泡沫塑料成型、片材成型、吹塑成型或类似成型。
它是由丙烯基聚合物或类似物实现的,其特点是满足以下要求(i)至(vi)。
要求 (i):MFR 为 0.1 克/10 分钟至 100 克/10 分钟。
要求(ii):GPC 的 Q 值为 3.5 至 10.5。
要求(iii):在 GPC 得出的分子量分布曲线中,分子量等于或大于 2,000,000 的组分所占比例等于或大于 0.4%,小于 10%。
要求 (iv):在 ODCB 的升温洗脱分馏中,在温度等于或低于 40°C 时洗脱的组分等于或小于 3.0%(按重量计)。
要求 (v):用 13C-NMR 测量的同素异形三聚体分数 (mm) 等于或高于 95%。
要求 (vi):在测量延伸粘度时,应变硬化度 (λmax)等于或高于 6.0。