Method for producing naphthalene carboxylic acid amide compound
申请人:Wakamori Hiroyuki
公开号:US20080045720A1
公开(公告)日:2008-02-21
The present invention provides a method for producing a naphthalenecarboxylic acid amide compound represented by formula [1] comprising, reacting a naphthalenecarboxylic acid halide compound represented by formula [2] with ammonium acetate in a solvent having an ether bond.
According to the method of the present invention, a naphthalene carboxylic acid amide compound can be obtained at high yield and at low cost.
Poly(ester-amide) capable of forming an anisotropic melt phase derived from 6-hydroxy-2-naphthoic acid, dicarboxylic acid and aromatic monomer capable of forming an amide linkage
申请人:CELANESE CORPORATION
公开号:EP0053940A1
公开(公告)日:1982-06-16
A melt processable poly(ester-amide) which is capable of forming an anisotropic melt phase is provided. The poly(ester-amide) of the present invention consists essentially of the recurring units (a) 6-oxy-2-naphthoyl moiety, (b) aryl dicarboxyl moiety or trans-1,4-dicarboxycyclohexane moiety, (c) an aromatic moiety capable of forming an amide linkage in the polymer and (d) optionally, dioxyaryl moiety in the proportions indicated. Preferably, the aromatic moiety capable of forming an amide linkage is p-aminophenol or p-phenylene-diamine. The resulting poly(ester-amide) exhibits a melting temperature below 400°C., preferably below 350°C. The poly(ester-amide) of the present invention is preferably formed by a melt polymerisation technique.
Polyester of 6-hydroxy-4-naphthoic acid, 4-hydroxy benzoic acid, 1-4-cyclohexanedicarboxylic acid, and aromatic diol capable of readily undergoing melt processing to form articles possessing high impact properties
申请人:CELANESE CORPORATION
公开号:EP0071447A1
公开(公告)日:1983-02-09
A novel polyester is provided which has been found to exhibit an optically anisotropic melt phase which enables it readily to undergo melt processing to form quality moulded articles possessing unusually high impact properties, etc. The polyester of the present invention contains recurring 6-oxy-2-naphthoyl, 4-oxybenzoyl and 1,4-dicarboxycyclohexane moieties in addition to a moiety derived from an aromatic diol in the proportions indicated. The hydrogen atoms present upon the aromatic rings optionally may be at least partially substituted (as described). The polyester is capable of forming the desired anisotropic melt at a temperature below approximately 350°C., and in a particularly preferred embodiment at a temperature below approximately 320°C.
Polyester of 6-hydroxy-2-naphthoic acid, aromatic diol and 1,4-cyclohexanedicarboxylic acid capable of undergoing melt processing
申请人:CELANESE CORPORATION
公开号:EP0049615A1
公开(公告)日:1982-04-14
A novel polyester is provided which has been found to exhibit an optically anisotropic melt phase which enables it readily to undergo melt processing to form quality fibres, films, moulded articles, etc. The polyester of the present invention contains recurring 6-oxy-2-naphthoyl moieties in addition to moieties derived from at least one aromatic diol and trans-1,4-cyciohexanedicarboxylic acid in the proportions indicated. The hydrogen atoms present upon the rings of these moieties optionally may be at least partially substituted (as described). The polyester is capable of forming the desired anisotropic melt at a temperature below approximately 350=C., and in a particularly preferred embodiment at a temperature below approximately 320°C.
Poly(ester amide) derived from 6-hydroxy-2-naphthoic acid, another aromatic hydroxy acid, dicarboxylic acid and an aromatic monomer capable of forming an amide link
申请人:CELANESE CORPORATION
公开号:EP0074700A1
公开(公告)日:1983-03-23
A melt processable poly(ester-amide) which is capable of forming an anisotropic melt phase is provided. The poly(ester-amide) of the present invention consists essentially of the recurring units (a) 6-oxy-2-naphthoyl moiety, (b) other aromatic moiety derived from aromatic hydroxyacid, (c) carbocyclic dicarboxyl moiety, (d) aromatic moiety capable of forming an amide linkage in the polymer, and, optionally, (e) dioxyaryl moiety in the proportions indicated. Preferably, the moiety capable of forming an amide linkage is derived from p-aminophenol or p-phenylenediamine. The resulting poly(ester-amide) exhibits a melting temperature below 400°C., preferably below 350°C. The poly(ester-amide) of the present invention is preferably formed by a melt polymerisation technique.