Process for preparation of modified polyethylene terphthalate with improved barrier, mechanical and thermal properties and products thereof
申请人:ESTER INDUSTRIES LIMITED
公开号:US10174162B2
公开(公告)日:2019-01-08
The present invention relates to a copolyester having intrinsic viscosity greater than 0.50 dL/gm, comprises: terephthalate polyester composition; and a modified transparent polybutylene naphthalate, wherein the modified polybutylene naphthalate comprises naphthalene dicarboxylic acid, 1,4-butane diol, and isophthalic acid or monoethylene glycol or diethylene glycol or cyclohexane dimethanol or polyethylene naphthalate, nucleating agent, and a modified nanoclay.