The invention relates to a composition for thermoplastic composite material comprising:
30% to 60% by volume, preferentially 35% to 50% by volume, of a thermoplastic matrix comprising from 50% to 100% by weight of a semi-crystalline polyamide polymer and from 0% to 50% by weight of at least one additive and/or of at least one other polymer,
40% to 70% by volume, preferentially 50% to 65% by volume, of long reinforcing fibers (or of long fibrous reinforcement),
said thermoplastic matrix impregnating said long reinforcing fibers (or said long fibrous reinforcement),
said semi-crystalline polyamide polymer being:
a) a reactive composition comprising or consisting of at least one reactive polyamide prepolymer which is a precursor of said semi-crystalline polyamide polymer, or, as an alternative to a),
b) a nonreactive composition of at least one polyamide polymer, said composition being that of said thermoplastic matrix defined above,
and said reactive polyamide prepolymer of the composition a) and said polyamide polymer of the composition b) comprising or consisting of at least one BACT/XT copolyamide.
本发明涉及一种用于热塑性复合材料的组合物,其中包括
30% 至 60% (按体积计算),最好是 35% 至 50% (按体积计算)的热塑性基体,其中包括 50% 至 100% (按重量计算)的半结晶聚酰胺聚合物和 0% 至 50% (按重量计算)的至少一种添加剂和/或至少一种其它聚合物、
40% 至 70% 的长增强纤维(或长纤维增强材料)(以体积计),最好是 50% 至 65%、
所述热塑性基质浸渍所述长增强纤维(或所述长纤维增强材料)、
所述半结晶聚酰胺聚合物为:
a) 反应性组合物,包括或由至少一种反应性聚酰胺预聚物组成,该预聚物是所述半结晶聚酰胺聚合物的前体,或者,作为 a) 的替代品、
b) 至少一种聚酰胺聚合物的非反应性组合物,所述组合物为上述热塑性基体、
组合物 a)中的反应性聚酰胺预聚物和组合物 b)中的聚酰胺聚合物包括至少一种
BACT/XT 共聚酰胺。