An explosive suitable for low energy initiation is made by coating epsilon structure one to five micron crystals of CL-20 with a polymeric binder where the polymeric binder is one to three percent by weight of the coated crystals and a method of applying such polymeric binders by either a slurry method or an alternate method of using a nonaqueous liquid to suspend CL-20 crystals then adding a lacquer of polymeric binder.
一种适用于低能量起爆的爆炸物是通过在ε结构的 1 至 5 微米 C
L-20 晶体上涂覆聚合粘合剂制成的,其中聚合粘合剂占涂覆晶体重量的 1%至 3%,涂覆聚合粘合剂的方法可以是浆料法,也可以是使用非
水性液体悬浮 C
L-20 晶体然后加入聚合粘合剂漆的替代方法。