日期:1996.4.30
temperature (Tp) is 50 °C; an increase of Tp decreases A, SY, and molecular weight (MW) of s-PS. Benz[e]IndTiCl3 (6a) as well as the 2-methyl (6b) and 1,2,3-trimethyl (11) derivatives have been synthesized. Complexes 6a/MAO and 6b/MAO have exceedingly high values of A ≈ 1.8 × 108 g of PS/(mol of Ti·mol of styrene·h) for a turnover rate of 450 s-1, SY over 92%, and MW ≈ 5 × 105. These parameters were only
描述了八种新型催化剂前体的合成,并将它们在甲基铝氧烷(MAO)活化时对间同苯乙烯聚合的催化作用与IndTiCl 3进行了比较。苯基取代以1,3-Ph 2 Ind <2-PhInd <1-PhInd的顺序增加聚合活性(A);间规聚苯乙烯(s -PS)的收率(SY)观察到相反的趋势。最佳聚合温度(T p)为50°C;T p的增加会降低A- SY和s -PS的分子量(MW)。奔驰[ e ] IndTiCl 3(6a)以及2-甲基(6b)和1,2,3-三甲基(11)衍生物已经合成。配合物6a / MAO和6b / MAO的A≈1.8×10 8 g PS /(Ti摩尔·苯乙烯·h摩尔)的极高值,周转率为450 s - 1,SY超过92%, MW≈5×10 5。这些参数在T p = 100°C时仅略有降低,表明其具有非常高的热稳定性和催化活性。这些催化剂前体在溶液中对空气和水分的稳定作用长达48小时,并在固态中无限稳定。虽然11