A cross-linked rubber product is obtained by cross-linking an acrylic elastomer composition containing an acrylic elastomer obtained by copolymerization of an acrylate and a cross-linking site monomer. The molar fraction of an oxygen atom (a) in the acrylic elastomer is 11.3 mol% or less, the molar fraction of a nitrogen atom (b) in the acrylic elastomer is 0.5 mol% or less, and a volume change is from -3 to 6% when the cross-linked rubber product is dipped in distilled water at 80°C for 200 hours.
一种交联橡胶产品是通过交联
丙烯酸弹性体组合物获得的,该组合物含有通过
丙烯酸酯和交联位点单体共聚获得的
丙烯酸弹性体。
丙烯酸弹性体中氧原子的摩尔分数(a)为 11.3 摩尔%或更少,
丙烯酸弹性体中氮原子的摩尔分数(b)为 0.5 摩尔%或更少,当交联橡胶制品在 80°C 的蒸馏
水中浸泡 200 小时时,体积变化为-3%至 6%。