A polyamide resin composition comprising:
[I] 100 parts by weight of a polyamide resin (A), and
[II] 5 to 200 parts by weight of a graft-modified ethylene/α-olefin random copolymer (B) obtainable by graft-modifying an ethylene/α-olefin random copolymer of ethylene and an α-olefin of 6 to 20 carbon atoms with an unsaturated carboxylic acid or a derivative thereof and having a graft quantity of 0.01 to 10% by weight based on the weight of the ethylene/α-olefin random copolymer before graft modification,
wherein the ethylene/α-olefin random copolymer (B) before the graft modification has the following properties:
(a) the content of the α-olefin of 6 to 20 carbon atoms is 6 to 25% by mol; and
(b) the intrinsic viscosity (η), as measured in decalin at 135°C, is 0.5 to 5.0 dl/g.
聚酰胺
树脂组合物,包括
按重量计,[I] 100 份聚酰胺
树脂(A),和
[II] 5 至 200 份(按重量计)接枝改性
乙烯/α-烯烃无规共聚物 (B),可通过接枝改性
乙烯和 6 至 20 个碳原子的α-烯烃与不饱和
羧酸或其衍
生物的
乙烯/α-烯烃无规共聚物,其接枝量为 0.01 至 10%(按接枝改性前
乙烯/α-烯烃无规共聚物的重量计)、
其中接枝改性前的
乙烯/α-烯烃无规共聚物(B)具有以下特性:
(a) 6 至 20 个碳原子的 α-烯烃含量为 6 至 25%(摩尔);以及
(b) 在 135°C 的
癸醛中测得的固有粘度 (η)为 0.5 至 5.0 分升/克。