To provide a new method for producing a composition containing a hardly water-soluble aromatic compound, the composition having outstanding hardly water-soluble aromatic compound.
A method for producing a composition containing a hardly water-soluble aromatic compound, comprising:
Step (1) of obtaining a hardly water-soluble aromatic compound solution 1, Step (1) comprising Step (1-1) of preparing a material for heating comprising (A) a hardly water-soluble aromatic compound, (B) a polyol, and (C) an aqueous medium, and Step (1-2) of obtaining a heated solution containing a hardly water-soluble aromatic compound by heating the material for heating at normal pressure at a temperature of less than 100°C; and
Step (2) of obtaining a hardly water-soluble aromatic compound solution 2 by adding water to the hardly water-soluble aromatic compound solution 1 such that the hardly water-soluble aromatic compound solution 2 has a concentration of the (A) hardly water-soluble aromatic compound above a saturation solubility at 25°C, wherein, in Step (1), a content of a surfactant in the material for heating is 0.1 mass% or less and a content of the (A) hardly water-soluble aromatic compound in the material for heating is below a saturation solubility of the (A) hardly water-soluble aromatic compound in a solvent having the same composition at 25°C.
提供一种生产含有难溶于
水的芳香族化合物的组合物的新方法,该组合物具有突出的难溶于
水的芳香族化合物。
一种生产含有难溶于
水的芳香化合物的组合物的方法,包括
步骤(1)获得难溶于
水的芳香族化合物溶液1,步骤(1)包括步骤(1-1)制备由(A)难溶于
水的芳香族化合物、(B)多元醇和(C)
水介质组成的加热用材料,以及步骤(1-2)通过在常压下以低于 100°C 的温度加热加热用材料,获得含有难溶于
水的芳香族化合物的加热溶液;以及
步骤 (2) 通过向难溶于
水的芳香族化合物溶液 1 中加
水,使难溶于
水的芳香族化合物溶液 2 中 (A) 难溶于
水的芳香族化合物的浓度高于 25°C 时的饱和溶解度,获得难溶于
水的芳香族化合物溶液 2,其中,在步骤 (1) 中,加热用材料中表面活性剂的含量为 0.1 质量%或更低,且加热材料中(A) 难溶于
水的芳香族化合物的含量低于(A) 难溶于
水的芳香族化合物在 25°C 时在成分相同的溶剂中的饱和溶解度。