The present invention provides an aromatic polycarbonate resin having high fluidity and thin-wall moldability as well as excellent transparency, impact strength, and bending resistance; a polycarbonate resin composition containing it; and a method for producing a molded article by injection molding thereof. This object is achieved by an aromatic polycarbonate resin containing a carbonate structural unit (A) represented by Formula (1) and a carbonate structural unit (B) represented by Formula (2), which aromatic polycarbonate resin satisfies the following: (i) the flow value (Q value) as measured using a Koka flow tester according to Appendix C of JIS (1999) K7210 at 240° C. at 160 kgf/cm2 is not less than 6 (unit: 10−2 cm3/sec.); and (ii) the glass transition temperature (Tg) is 90 to 145° C.
本发明提供了一种具有高流动性、薄壁成型性以及优异的透明度、冲击强度和抗弯曲性的芳香族聚
碳酸酯
树脂;一种含有该
树脂的聚
碳酸酯
树脂组合物;以及一种通过注塑成型生产成型品的方法。该目标是通过一种芳香族聚
碳酸酯
树脂来实现的,该芳香族聚
碳酸酯
树脂含有由式(1)表示的
碳酸酯结构单元(A)和由式(2)表示的
碳酸酯结构单元(B),该芳香族聚
碳酸酯
树脂满足以下条件:(i) 在 240 摄氏度、160 千克力/平方厘米条件下,使用符合 JIS (1999) K7210 附录 C 的 Koka 流量测试仪测得的流量值(Q 值)不小于 6(单位:10-2 立方厘米/秒);以及 (ii)
玻璃化转变温度(Tg)为 90 至 145 摄氏度。