A vulcanizable rubber composition is described comprising:
a) a polymer base in which reinforcing fillers are homogeneously dispersed including:
a1) a first modified copolymer obtainable by polymerization of at least one conjugated diolefin with at least one vinyl aromatic hydrocarbon in the presence of an initiator comprising at least one organic metal group and subsequent modification by reacting the so obtained intermediate copolymer with a compound comprising functional groups capable of reacting with the organic metal groups of the copolymer and derived from the initiator, said first copolymer having a glass transition temperature comprised between 0° and -80°C, and comprising a total quantity of vinyl aromatic hydrocarbon comprised between 5% and 50% by weight to the total weight of the same;
a2) a second copolymer obtainable by polymerization of at least one conjugated diolefin with at least one vinyl aromatic hydrocarbon, said second copolymer having a glass transition temperature comprised between 0° and -80°C, and comprising a total quantity of vinyl aromatic hydrocarbon comprised between 5% and 50% by weight to the total weight of the same;
b) a first carbon black-based reinforcing filler in such a quantity that the volume electrical resistivity of the vulcanized rubber composition does not exceed 10-6 Ohmxcm;
c) a second silica-based reinforcing filler in such a quantity that the sum of said first and said second reinforcing fillers is comprised between 50 and 100 parts by weight per 100 parts by weight of polymer base.
所述可
硫化橡胶组合物包括
a) 聚合物基料,其中均匀分散有增强填料,包括
a1) 第一种改性共聚物,可通过至少一种共轭二烯烃与至少一种
乙烯基芳香烃在含有至少一种有机
金属基团的
引发剂存在下进行聚合反应而获得,随后通过将获得的中间共聚物与一种含有能与共聚物的有机
金属基团反应的官能团并来自
引发剂的化合物进行反应而进行改性,所述第一种共聚物的
玻璃化温度介于 0° 至 -80°C 之间,
乙烯基芳香烃的总量占其总重量的 5%至 50%(按重量计);
a2) 通过至少一种共轭二烯烃与至少一种
乙烯基芳香烃聚合得到的第二种共聚物,所述第二种共聚物的
玻璃化温度在 0° 至 -80°C 之间,
乙烯基芳香烃的总量占其总重量的 5%至 50%;
b) 第一种
炭黑基补强填料,其用量应使
硫化橡胶组合物的体积电阻率不超过 10-6 欧姆xcm;
c) 第二种以
二氧化硅为基础的补强填料,其用量为每 100 重量份的聚合物基料中,上述第一种和第二种补强填料的总和在 50 至 100 重量份之间。