A reaction of activated silicon with alcohols in an autoclave at 240—270 °C was studied. It was found that primary alcohols form tetraalkoxysilanes Si(OR)4 with high selectivity (up to 97%), while the secondary PriOH gave a mixture of compounds HSi(OPri)3, Si(OPri)4, HSi(OPri)2OSi(OPri)2H, HSi(OPri)2OSi(OPri)3, and Si(OPri)3OSi(OPri)3 with the predominance of trialkoxysilane (up to 67%). Carrying out
研究了活性硅与醇在 240-270 °C 的高压釜中的反应。发现伯醇以高选择性(高达 97%)形成四烷氧基硅烷 Si(OR)4,而仲 PriOH 生成化合物 HSi(OPri)3、Si(OPri)4、HSi(OPri)2OSi( OPr)2H、HSi(OPri)2OSi(OPri)3 和 Si(OPri)3OSi(OPri)3,主要是三烷氧基硅烷(高达 67%)。在指定条件下进行反应具有实验简单、试剂易得、硅转化率高、产物分离收率好等优点。