cocrystal phase in the milled sample. The activation energy of the thermal decomposition of CL-20/RDX is 206.49 kJ mol−1 higher than that of raw RDX. DSC-IR analysis showed that the thermolysis of CL-20/RDX produces a large amount of CO2 and N2O and a small amount of H2O, NO2 and NO. The mechanical sensitivity of CL-20/RDX is very low. In impact sensitivity tests with a 5 kg hammer, the special height
通过研磨 2,4,6,8,10,12-hexanitro-2,4,6,8,10,12-hexaazaisowurtzitane (C
L-20) 和 hexahydro-1,3,5-trinitro-1,3,5 -三嗪(RDX),以该原料制备平均粒径为141.6 nm的纳米C
L-20/RDX co/混晶炸药,并用扫描电镜(
SEM)对co/混晶进行表征,透射电子显微镜 (
TEM)、X 射线衍射 (XRD)、拉曼光谱、红外 (IR) 光谱、X 射线光电子能谱 (XPS)、差示扫描量热法 (
DSC) 和在线热红外光谱法 (
DSC-IR)技术; 此外,还测试了样品的冲击、摩擦和热敏感性。结果表明,经研磨后,
钴/混晶炸药的形貌接近球形,粒径呈正态分布。研磨后的样品显示出与原料相同的分子结构和表面元素,但 XRD 测试表明 C
L-20/RDX 具有新的晶相,拉曼和 IR 光谱补充证实了共晶相的存在。磨碎