申请人:DAINIPPON INK AND CHEMICALS, INC.
公开号:EP0765913A1
公开(公告)日:1997-04-02
The present invention provides a process for the preparation of a biodegradable lactic acid-based polyester composition excellent in thermal stability, storage stability, flexibility, heat resistance, mechanical and physical properties and moldability which comprises kneading a lactic acid-based polyester and a polyester consisting of dicarboxylic acid component(s) and diol component(s) with a chelating agent, an acidic phosphoric acid ester, a molecular weight increasing agent, etc., and then devolatilizing the kneaded mixture. The present invention also provides a molding process of the foregoing lactic acid-based polyester composition. A process for the preparation of a lactic acid-based polyester composition is provided, which comprises melt-kneading a lactic acid-based polyester (A), a polyester (B) consisting of dicarboxylic acid component(s) and diol component(s) and a chelating agent and/or acidic phosphoric acid ester (C) in an amount such that the weight ratio (A)/(B) is from 99/1 to 10/90 and the proportion of (C) is 0.001 to 5 parts by weight based on 100 parts by weight of the sum of (A) and (B). A process for molding a lactic acid-based polyester composition is also provided, which comprises kneading a lactic acid-based polyester (A) and a polyester (B) consisting of dicarboxylic acid component(s) and diol component(s) with a chelating agent and/or acidic phosphoric acid ester (C), and then molding the material.
本发明提供了一种在热稳定性、储存稳定性、柔韧性、耐热性、机械和物理性能以及成型性方面具有优异性能的可生物降解的乳酸基聚酯组合物的制备工艺,该工艺包括将乳酸基聚酯和由二羧酸组分和二元醇组分组成的聚酯与螯合剂、酸性磷酸酯、分子量增加剂等进行捏合,然后将捏合后的混合物脱胶。本发明还提供了前述乳酸基聚酯组合物的成型工艺。本发明提供了一种乳酸基聚酯组合物的制备工艺,该工艺包括熔融捏合乳酸基聚酯 (A)、由二羧酸组分和二元醇组分组成的聚酯 (B) 以及螯合剂和/或酸性磷酸酯 (C),其用量使得(A)/(B)的重量比为 99/1 至 10/90,(C)的比例为 0.001至5份重量比,以100份重量比的(A)和(B)之和为基准。还提供了一种成型乳酸基聚酯组合物的工艺,包括将乳酸基聚酯(A)和由二羧酸组分和二元醇组分组成的聚酯(B)与螯合剂和/或酸性磷酸酯(C)捏合,然后将材料成型。