Coupling agents have been widely used to retard the sintering of silver paste and minimize co-firing defects due to densification mismatch between silver and dielectrics. The thermal-decomposition and crystallization behavior of the coupling agent is a subject of great concern. To elucidate what is responsible for the oxidation, Ti organometallic compounds were calcined at different temperatures (350,400, 500, 600 degrees C) for 2 h and the crystallization behavior was determined by X-ray diffraction (XRD). The activation energy for crystallization of coupling agents was studied by using isothermal methods. According to the quantitative XRD method, the values calculated by the Johnson-Mehi-Avrami equation are 134.9 kJ mol(-1). The growth morphology parameters are 1.061, 0.915, 1.016 respectively. Combining the results of DTA, XRD and TEM, it is found that formation of nanocrystallized titania accompanies the combustion of organometallic compounds. (C) 2009 Elsevier B.V. All rights reserved.