A cross-linkable nitrile rubber composition comprising a highly saturated nitrile rubber (A) containing α,β-ethylenically unsaturated nitrile monomer units in a ratio of 10 to 60 wt% and having an iodine value of 120 or less, a master batch (B) containing an ethylene-vinyl acetate copolymer (b1) having a melt flow rate measured under a load of 21.18N at 190°C of 0.5 to 1000 g/10 min. and containing vinyl acetate monomer units in a ratio of 5 to 50 wt% and an organic staple fiber (b2) having an average fiber length of 0.1 to 12 mm, and a cross-linking agent (C), wherein a ratio of the ethylene-vinyl acetate copolymer (b1) and the organic staple fiber (b2) in the master batch (B) is, in terms of a weight ratio of "ethylene-vinyl acetate copolymer (b1) :organic staple fiber (b2)", 30:70 to 80:20 is provided.
一种可交联
丁腈橡胶组合物,包括一种高饱和
丁腈橡胶 (A),其中α,β-
乙烯基不饱和
丁腈单体单元的比例为 10 至 60 wt%,
碘值为 120 或更低;一种母料 (B),其中
乙烯-
醋酸乙烯共聚物 (b1),其在 190°C 时的载荷为 21.18N 的条件下测得的熔体流动速率为 0.5 至 1000 g/10min,其中
醋酸乙烯单体单元的比例为 5 至 50 wt%;以及一种有机短纤维 (b2),其平均纤维长度为 0.
乙烯-
醋酸乙烯共聚物 (b1)在 190°C、21.18N 载荷下测得的熔体流动速率为 0.5 至 1000 克/10 分钟,其中
醋酸乙烯单体单元的比例为 5 至 50 wt%,有机短纤维 (b2) 的平均纤维长度为 0.其中母料 (B) 中
乙烯-
醋酸乙烯共聚物 (b1) 和有机短纤维 (b2) 的重量比为 "
乙烯-
醋酸乙烯共聚物 (b1) :有机短纤维 (b2)",即 30:70 至 80:20。