The invention concerns a process for preparing composite resin particles having the so-called semi-IPN (inter penetration network) structure, in which linear thermoplastic polymer chains get entangled with a crosslinked polymer core through partial or thorough penetration. This method is important in that both of the chain polymer and core polymer are freely selected from various resins.
Composite resin particles prepared by dispersing in an aqueous medium a uniform mixture of
(A) a crosslinked structure-forming component having a number average molecular weight of about 180 to 1,000,000 selected from a resin having both dispersive power and cross linking property or a combination of two organic compounds each bearing mutually reactive functional groups which are required for the formation of crosslinked high molecular weight compound when said two compounds are reacted with each other, at least one of said organic compounds having dispersive power, and
(B) a non -crosslinking thermoplastic resin which is not reactive with said (A) component,
effecting a crosslinking of the crosslinked structure-forming components in the dispersed particles, and removing the aqueous medium.
本发明涉及一种制备具有所谓半 I
PN(相互渗透网络)结构的复合
树脂颗粒的工艺, 在这种结构中,线性热塑性聚合物链通过部分或完全渗透与交联聚合物芯缠结在一起。这种方法的重要之处在于,链聚合物和芯聚合物都可以从各种
树脂中自由选择。
复合
树脂颗粒的制备方法是将下列物质的均匀混合物分散在
水介质中。
(A) 交联结构形成组分,其平均分子量在 180-1,000,000 之间,该组分可选自同时具有分散能力和交联特性的
树脂,或两种有机化合物的组合,每种有机化合物都带有相互反应的官能团,当所述两种化合物相互反应时,需要这些官能团形成交联的高分子量化合物,所述有机化合物中至少有一种具有分散能力,和
(B) 非交联热塑性
树脂,它与所述 (A) 组分不发生反应、
使分散颗粒中的交联结构形成成分发生交联,并除去
水介质。