日期:1966.6
been prepared from the corresponding chlorosilanes and vinylmagnesium chloride. In these compounds, intense absorption maxima were observed in the ultraviolet region, and both the λmax and e increased with an increase in the chain length. Nuclear magnetic resonance and infrared data are also recorded here. Free radical copolymerizations were carried out with styrene and with acrylonitrile, and the monomer