A modified microwave-assisted polyol method was applied to prepare nanoparticulate ceramic powders of different oxides, i.e. Gdsub 2}Osub 3}, AlO(OH) (boehmite) and TiOsub 2}. Due to the good dielectric properties of the utilised solvents, such as ethylene glycol, diethylene glycol and 1,4 butanediol, a significant decrease in reaction time was achieved under microwave heating. In the case of AlO(OH)