申请人:Sakai Chemical Industry Co., Ltd.
公开号:US06306787B1
公开(公告)日:2001-10-23
The invention provides nickel hydroxide secondary particles comprising agglomerates of primary particles of nickel hydroxide in the shape of a triangular prism or a triangular plate having a surface or a outer face in the form of a substantially equilateral triangle each side of which substantially equilateral triangle has a length of 1 to 10 &mgr;m. The invention further provides lithium nickel composite oxide secondary particles comprised of agglomerates of primary particles having a large particle diameter by mixing the nickel hydroxide secondary particles with a lithium compound and sintering the resulting mixture at a temperature of 600° C. to 1000° C. in an oxidative atmosphere.