申请人:Toray Industries, Inc.
公开号:EP2666633A1
公开(公告)日:2013-11-27
[Problem] To provide: a layered polyester film which shows highly long-lasting adhesion of various kinds to hardcoat layers having various functions represented by a UV-absorbing function, etc. and which shows satisfactory appearance properties due to diminished interference unevenness; and a hardcoat film. [Solution] A Laminated polyester film which comprises a substrate polyester film (layer S) with at least one surface being laminated with a lamination layer (layer C) comprising a polyester resin as a primary component, the surface of the lamination layer (layer C) having a wetting tension of 35-45 mN/m and the polyester resin contained in the lamination layer (layer C) meeting the following requirements (a) to (c). (a) The lamination layer (layer C) contains polyesters (A) having a glass transition temperature (Tg) of 110-140°C and polyesters (B) having a glass transition temperature (Tg) of 40-90°C. (b) At least either polyesters (A) or polyesters (B) contains both a monomer having a sulfonic acid component and a monomer having a multivalent, i.e., tri- or higher-valent, carboxylic acid component, and (c) The mixing ratio between polyesters (A) and polyesters (B) is from 10/90 to 60/40.
[问题]提供:一种分层聚酯薄膜,它与具有各种功能(如紫外线吸收功能等)的硬涂层具有高度持久的粘合力,并且由于干涉不均匀度降低而具有令人满意的外观特性;以及一种硬涂层薄膜。[解决方案] 一种层压聚酯薄膜,它包括基底聚酯薄膜(层 S),其至少一个表面与层压层(层 C)层压,层压层(层 C)的主要成分是聚酯树脂,层压层(层 C)表面的润湿张力为 35-45 mN/m,层压层(层 C)所含的聚酯树脂符合以下要求(a)至(c)。(a) 层压层(层 C)包含玻璃化转变温度(Tg)为 110-140°C 的聚酯(A)和玻璃化转变温度(Tg)为 40-90°C 的聚酯(B)、(c) 聚酯(A)和聚酯(B)的混合比例为 10/90 至 60/40。