Disclosed is a (meth)acrylate polymer having a volume average primary particle size of 0.520 to 3.00 μm, a peak temperature of tan δ in the range of −100 to 0° C., determined with dynamic viscoelasticity measurement, of −40° C. or below, a peak height of tan δ in the range of −100 to 0° C., determined with dynamic viscoelasticity measurement, of 0.300 or more, and an acetone-insoluble component of 99% by mass of more.
This polymer has excellent dispersibility of primary particles in a resin, excellent storage stability of a resin composition obtained, and excellent insulating properties and reduction in elastic modulus of a molded article obtained.
本发明涉及一种(甲基)
丙烯酸酯聚合物,其体积平均主粒子大小为0.520至3.00μm,tanδ在−100至0℃范围内的峰值温度,通过动态粘弹性测量确定为−40℃或更低,tanδ在−100至0℃范围内的峰值高度,通过动态粘弹性测量确定为0.300或更高,且
丙酮不溶组分为质量的99%以上。该聚合物具有在
树脂中主粒子的优异分散性,所得
树脂组合物的优异储存稳定性,以及所得成型品的优异绝缘性和弹性模量降低。